™Log inStart free
    INBDE subjectClinical dentistryFree to read

    INBDE Dental Materials

    A one-page high-yield review of dental materials for the INBDE, and 3 practice questions with every answer explained.

    Written from open sources: every line of the review comes from DentPrep's Dental Materials guide, and every question here ties each claim to a quote from its source and was answered blind by a second AI model. None comes from the live exam.

    See the questions

    No account needed for the test · Free account · No card

    On this page

    What the INBDE tests in Dental Materials

    The JCNDE doesn't publish a list by subject. It writes the INBDE to its clinical content areas. These are the content areas DentPrep maps most dental materials questions to:

    1. 30Restore tooth function, structure, and esthetics by replacing missing and defective tooth structure, while promoting soft and hard tissue health.
    2. 56Communicate case design to laboratory technicians and evaluate the resultant restoration or prosthesis.
    3. 38Manage the oral esthetic needs of patients.

    DentPrep's checklist for Dental Materials has 19 topics:

    • Structure of matter
    • Mechanical properties
    • Physical, thermal and optical properties
    • Biocompatibility and safety
    • Adhesion to enamel and dentin
    • Resin composite
    • Light curing
    • Glass ionomer and its hybrids
    • Dental amalgam
    • Liners, bases and pulp-protection materials
    • Preventive and esthetic agents
    • Luting cements
    • Impression materials
    • Gypsum products
    • Alloys, casting and wire
    • Dental ceramics
    • Polymers for dentures and provisionals
    • Implant and endodontic materials
    • Waxes, abrasives and finishing

    Dental Materials high-yield review

    The cheat sheet from DentPrep's Dental Materials notes, as it is in the app. Each line names the guide section it comes from.

    Structure and properties

    • Glass = amorphous (random atoms); ceramic = crystalline grains, a little glass at grain boundaries; glass-ceramic = crystals in a glassy matrix. Guide: Glass, crystal and glass-ceramic
    • Leucite CTE ~17 × 10−6 K−1 against feldspar glass ~8: mixing them gives 12−14 to match a metal framework. Guide: Glass, crystal and glass-ceramic
    • Dislocations carry plastic deformation: bonds break and reform a row at a time. Guide: Metals: dislocations and plastic flow
    • Tg rises with cure: almost 50 °C higher when exposure went from 40 to 120 s. Guide: Polymers: the glass transition
    • Elastic modulus = elastic stress ÷ elastic strain (stiffness); flexibility is its reciprocal. Guide: The stress-strain curve
    • Past the elastic limit, unloading leaves permanent strain; yield strength = the stress at a set amount of plastic strain. Guide: The stress-strain curve
    • Resilience = elastic energy to yield (given back); toughness = total area under the curve; ductility = % elongation. Guide: Ductility, brittleness, resilience and toughness
    • Fracture toughness (KIc) = resistance to an existing crack's growth, tested with a crack of known size; zirconia's comes from transformation. Guide: Fracture toughness and crack stopping
    • Brittle materials: tensile strength by the diametral test, a cylinder compressed across its diameter. Guide: Brittle materials and the diametral tensile test
    • Fatigue can break a metal far below its ultimate strength, even below yield; some materials have a fatigue (endurance) limit. Guide: Fatigue
    • Vickers and Knoop: a diamond indenter; a composite's surface hardness tracks its cure. Guide: Hardness
    • Conductivity: polymers < ceramics < metals; zirconia 2.5–2.8, lithium disilicate 5.2, alumina 30 W/m·K. Guide: Thermal conductivity and diffusivity
    • Composite and glass ionomer conduct about like tooth; amalgam x20, gold x300; harm possible above a 5.5 °C pulp rise (42.4°C). Guide: Thermal conductivity and diffusivity
    • Changing temperature: diffusivity decides (density and heat capacity too). Guide: Thermal conductivity and diffusivity
    • Amalgam: higher expansion than tooth and a conductor, so thermal cycling opens its margin; resin expands more but insulates. Guide: Thermal expansion and the margin
    • Water sorption stains, weakens and attacks the resin-filler bond; solubility releases residual monomer. Guide: Water sorption and solubility
    • Hue = which color; value = light or dark; chroma = how vivid. Select value, then chroma, then hue. Guide: Color: hue, value, chroma and metamerism
    • Metamerism: illuminant (light), geometric (angle), observer (color blindness). Guide: Color: hue, value, chroma and metamerism
    • Galvanism: dissimilar metals interacting through saliva; one review cites <10 µA not critical, 20 µA pain, 75 µA to 100 µA irritation. Guide: Corrosion and galvanic current
    • One review's least corrosion-resistant: amalgam and nickel-chromium (Ni up to 5.22 µg/cm2/day); titanium's dioxide film; passivation. Guide: Corrosion and galvanic current
    • Lichenoid contact lesion: type IV to mercury, months to years, beside the amalgam, usually one side; gingiva and palate rarely. Guide: Allergy and the lichenoid contact lesion
    • Patch test held 48 hours, read at 48 and 72 hours; late readings at 10–14 days can catch missed reactions. Guide: Allergy and the lichenoid contact lesion
    • Pulp inflammation under a restoration: mainly bacteria via microleakage; undercured resin releases more monomer. Guide: Biocompatibility: what harms the pulp, and how it is judged
    • Bis-GMA derives from BPA; BPA found in saliva and urine after treatment; MTT is in ISO 10993. Guide: Biocompatibility: what harms the pulp, and how it is judged
    • Metal tattoo: metal ground off in crown work, in the gingival connective tissue (melanin is in the epithelium); radiographs show it only occasionally; a new crown does not clear it: remove the debris in stages, or graft. Guide: The metal tattoo

    Amalgam

    • About half mercury, half alloy powder of silver, tin and copper; zinc up to 1% as a scavenger. Guide: Amalgam: composition and setting
    • Phases: γ = Ag3Sn (particle cores), γ1 = Ag2Hg3 (the matrix), γ2 = tin-mercury (weakest, corrodes), η′ = Cu6Sn5. Guide: Amalgam: composition and setting
    • No bond to tooth, so microleakage at first. Guide: Amalgam: composition and setting
    • Low-copper about 6% Cu; high-copper needs a minimum of 12 wt% Cu to eliminate γ2. Guide: High-copper amalgam and gamma-2
    • Copper takes tin into Cu6Sn5: less γ2, corrosion, tarnish and creep; not dispersion hardening. Guide: High-copper amalgam and gamma-2
    • High-copper amalgams survive longer; leading failure bulk fracture (4.6%). Guide: High-copper amalgam and gamma-2
    • Eames: 1:1 mercury to alloy. Guide: Amalgam: handling, moisture and zinc
    • Zinc + moisture during condensation = delayed expansion (hydrogen gas); a zinc-free alloy avoids that reaction. Guide: Amalgam: handling, moisture and zinc
    • High compressive strength, low creep, minimal dimensional change; margins seal with corrosion products. Guide: Amalgam: properties in service
    • FDA 2020: high-risk groups (pregnant, planning pregnancy, nursing, children under six, neurological or kidney disease, mercury allergy) avoid new amalgam where possible. Guide: Amalgam and mercury: the FDA's 2020 recommendations
    • Amalgams in good condition are not removed unless medically necessary: removal raises mercury vapor and loses tooth. Guide: Amalgam and mercury: the FDA's 2020 recommendations
    • Mercury's vapor pressure rises fast with heat: polishing and removal release the most; inhaled vapor is absorbed, oxidized to ionic mercury and bound to proteins (kidneys, CNS). Guide: Amalgam and mercury: the FDA's 2020 recommendations

    Resin composite

    • Bis-GMA: stiff, very viscous, less shrinkage; TEGDMA thins it but raises water sorption and lowers strength. Guide: Resin composite: the matrix and the initiator
    • UDMA viscosity about 100 times lower than Bis-GMA. Guide: Resin composite: the matrix and the initiator
    • Camphorquinone peaks at 468 nm and needs a tertiary amine; TPO about 380 nm (type I), less yellow. Guide: Resin composite: the matrix and the initiator
    • Silane (γ-MPTS) bonds filler to matrix and makes the interface more resistant to water. Guide: Resin composite: fillers and the silane
    • Macrofill 10–50 μm: wears, polishes poorly; microfill ≈40 nm: polishes, weak (low loading); hybrids balance. Guide: Resin composite: fillers and the silane
    • C-factor = bonded ÷ unbonded surface; high in a Class I box (≈ 5); thin increments lower each one's, oblique ones most. Guide: Polymerization shrinkage and the C-factor
    • Conventional composite: increments of 2 mm or less, each cured; bulk-fill: one increment of up to 4–5 mm, C-factor unchanged. Guide: Polymerization shrinkage and the C-factor

    Light curing

    • Radiant exposure (J/cm²) = irradiance (mW/cm²) × time (s) ÷ 1000; short boost modes can deliver less. Guide: Light curing
    • Polywave LED (violet ≈395–415 nm and blue ≈450–470 nm) when the initiator is unknown or type I. Guide: Light curing
    • Tip as close as possible to 0 mm; 2–4 mm already matters; the gingival floor of a Class II box is the high-risk zone. Guide: Light curing
    • Pulp threshold about 5.5 °C (Zach and Cohen; questioned as an absolute value); riskiest when curing the adhesive over thin dentin; eye protection for blue-violet light. Guide: Light curing
    • Curing heat: the light plus the resin's own exothermic reaction (C=C double bonds becoming single bonds). Guide: Light curing

    Glass ionomer and its hybrids

    • Polyalkenoic acid + basic fluoride alumino-silicate glass + water; acid-base set in 2–3 min, then maturation. Guide: Glass ionomer
    • Chemical bond: carboxylate to calcium; collagen not involved; failure usually cohesive. Guide: Glass ionomer
    • Fluoride: early burst, then slow diffusion; recharge declines with maturation. Guide: Glass ionomer
    • In acid, glass ionomer releases more fluoride, and hydroxyapatite takes it up, so more reaches the tooth's mineral. Guide: Glass ionomer
    • Protect from moisture for at least 24 hours (varnish or petroleum jelly); drying makes it chalky and cracked. Guide: Glass ionomer
    • RMGI: acid-base + polymerization (typically HEMA and camphorquinone); HEMA release lowers biocompatibility. Guide: Resin-modified glass ionomer and compomer
    • Compomer sets mainly by polymerization and is used with an adhesive. Guide: Resin-modified glass ionomer and compomer

    Adhesion

    • Enamel: 30–40% phosphoric acid, the gold standard; self-etch etches enamel less, so etch enamel selectively. Guide: Etching enamel
    • Etched dentin air-dried hard: collagen collapses and the resin infiltrates it poorly. Guide: Bonding to dentin and the hybrid layer
    • MMPs degrade poorly infiltrated hybrid layers in vitro; clinical studies report no benefit from chlorhexidine. Guide: Bonding to dentin and the hybrid layer
    • Etch-and-rinse removes the smear layer; self-etch incorporates it. Guide: Adhesive systems: etch-and-rinse, self-etch and universal
    • Best records: 3-step etch-and-rinse and 2-step self-etch; 1-step adhesives act as permeable membranes. Guide: Adhesive systems: etch-and-rinse, self-etch and universal
    • 10-MDP bonds ionically to calcium; phosphoric acid depletes dentin calcium, so etch the enamel selectively. Guide: Adhesive systems: etch-and-rinse, self-etch and universal
    • Self-etch by pH: ultra-mild ≥ 2.5, mild ≈ 2, intermediately strong 1–2, strong < 1. Guide: Adhesive systems: etch-and-rinse, self-etch and universal
    • Most universal adhesives under a self- or dual-cure core or cement need their dual-cure activator. Guide: Adhesive systems: etch-and-rinse, self-etch and universal

    Liners, bases and preventive agents

    • Liner: usually <0.5 mm, seals or treats; base: replaces missing dentin (bulk, undercuts); a suspension liner dries to a 20–25 µm film: no strength, no insulation. Guide: Liner, base and varnish
    • Bases under amalgam now only for deep cavities with a calcium hydroxide liner; liners showed no clinical benefit in 12 studies. Guide: Liner, base and varnish
    • Calcium hydroxide: hydroxyl ions, alkaline pH, antibacterial, signals tertiary dentin; weak and soluble; if used, only where remaining dentin ≤0.5 mm (one review), never on the margin. Guide: Calcium hydroxide liners
    • MTA: di- and tricalcium silicate + about 20% bismuth oxide; hydration → calcium silicate hydrate + calcium hydroxide; ProRoot sets in over two hours. Guide: Hydraulic calcium silicate cements: MTA and its successors
    • MTA's gray: bismuth oxide (worse with sodium hypochlorite); newer cements use zirconium oxide; Biodentine's calcium chloride speeds the set. Guide: Hydraulic calcium silicate cements: MTA and its successors
    • Eugenol hinders resin setting: RMGI, not ZOE, under composite; modified ZOE (20% PMMA, or EBA) for bases and temporaries. Guide: Zinc oxide-eugenol and the temporary fillings
    • Cavit: zinc oxide and calcium sulfate, expands as it absorbs water (14% linear in one study): seals, can crack walls. Guide: Zinc oxide-eugenol and the temporary fillings
    • SDF + hydroxyapatite → silver phosphate, yellow then black in light; potassium iodide right after → creamy white silver iodide, less stain. Guide: Silver diamine fluoride and potassium iodide
    • Carbamide peroxide × 0.36 = hydrogen peroxide (10% ≈ 3.6%), plus urea; peroxide oxidizes chromogen double bonds; metallic stains bleach poorly. Guide: Bleaching agents: hydrogen and carbamide peroxide
    • Residual oxygen after bleaching hinders resin bonding: a review cited deferring about two weeks. Guide: Bleaching agents: hydrogen and carbamide peroxide

    Luting cements

    • Non-adhesive: zinc phosphate, zinc oxide eugenol (mechanical interlocking only); chemically adhesive: polycarboxylate, glass ionomer; resin: micromechanical. Guide: Luting cements
    • Zinc phosphate: exothermic; unreacted acid at pH ±1.5 at seating, 3.5 at end of mixing, 6.7 after 24 hours; thin remaining dentin buffers less; varnish cuts retention up to 50%. Guide: Zinc phosphate
    • Polycarboxylate: chelates calcium; long polyacrylic chains stay out of the tubules (gentle even at 0.2 mm); 55 MPa; 2.5 min working time; never add liquid. Guide: Zinc polycarboxylate
    • RMGI absorbs water and expands: contraindicated under fragile all-ceramic crowns. Guide: Glass ionomer and resin-modified glass ionomer luting cements
    • Self-adhesive resin cement: acidic monomers (MDP), no separate etch; weaker bond, not for short crowns or veneers. Guide: Resin cements: adhesive and self-adhesive
    • One review: light-cure under 1.5 mm and veneers, dual 1.5–2.5 mm, self-cure for metal and opaque or thick (amines discolor); dual cure without light as low as 10.82% in one study. Guide: Curing a resin cement: light, self and dual
    • Before resin bonding: noneugenol provisional cement, every trace removed. Guide: Provisional cements and eugenol

    Impression materials

    • Alginate: trisodium phosphate takes calcium sulfate first (working time), then calcium alginate; air = syneresis, water = imbibition; damp gauze; one pour. Guide: Alginate
    • PVS: platinum catalyst, no by-product; latex sulfur poisons it; hydrogen bubbles a die poured early (defer one hour); surfactants make it wettable. Guide: Addition silicone (polyvinyl siloxane)
    • Condensation silicone releases alcohol (shrinks: pour promptly); polysulfide releases water. Guide: Condensation silicone and polysulfide
    • Polyether: rigid, absorbs water; immersion over 30 min changed it. Guide: Polyether
    • More filler, less shrinkage: thin light body for detail, putty or heavy body for bulk. Guide: Viscosity and the putty-wash

    Alloys, casting and wire

    • ADA: high noble ≥60% noble and ≥40% gold; noble ≥25%; predominantly base <25%. Guide: The ADA classification of casting alloys
    • Co-Cr: E 200–220 GPa (cpTi 110, Type IV gold 81–90): thinner sections; half gold's density; no Ni allergy or Be risk. Guide: Base-metal alloys: cobalt-chromium and nickel-chromium
    • Interdendritic shrinkage porosity: unfed solidification; worst at abrupt thickness changes; breaks clasps. Guide: Casting porosity in a cobalt-chromium framework
    • Metal-ceramic: chemical bond through the oxide (thin removed in baking, thick weak); porcelain contracts slightly less than metal → compression. Guide: The metal-ceramic bond
    • NiTi: austenite ⇄ martensite under stress = force plateau; shape set at 482 °C; heat from soldering destroys superelasticity. Guide: Nickel-titanium wire

    Ceramics

    • Glass-matrix (feldspathic, leucite, lithium disilicate), polycrystalline (zirconia), resin-matrix (softer, gentle on opposing teeth). Guide: The three classes of dental ceramic
    • Lithium disilicate: HF etch, then silane. Guide: Lithium disilicate and other glass-ceramics: etch and silane
    • HF on skin: undissociated HF penetrates, fluoride binds calcium and magnesium; deep, delayed injury with little to see; rinse, then calcium gluconate. Guide: Lithium disilicate and other glass-ceramics: etch and silane
    • Transformation toughening: tetragonal → monoclinic at the crack tip, +4–5% volume, compression. Guide: Zirconia: transformation toughening
    • LTD: moisture at low temperature ages 3Y-TZP; glaze protects, margins exposed; translucent zirconia: more yttria and cubic crystals, weaker. Guide: Zirconia: aging and translucent zirconia
    • Zirconia: no silica, so no HF or silane; air-abrade gently, then 10-MDP; after try-in air-abrade again (water, alcohol, phosphoric acid fail). Guide: Bonding to zirconia
    • Veneered zirconia chips in the veneer: 11.8% at 5 years (metal-ceramic 3.5%); hand-layered pores and veneer over 1.5 mm add to it; monolithic has no veneer. Guide: Veneered zirconia: chipping

    Polymers for dentures and provisionals

    • PMMA powder: beads, benzoyl peroxide, plasticizer, pigments; liquid: methyl methacrylate, a cross-linker, hydroquinone. Guide: PMMA: what it is and how it is activated
    • Heat cure (~9 h at 74 °C) converts more; cold cure (tertiary amine activator) fits better but leaves more monomer and discolors: trays, repairs, provisionals. Guide: PMMA: what it is and how it is activated
    • Sandy → stringy → doughy (pack the flask) → rubbery → stiff; low powder-to-liquid ratio, more shrinkage. Guide: Mixing and packing: the dough stage and shrinkage
    • Flask into boiling water: monomer boils (100.3 °C) → porosity; soak new dentures in water to lower residual monomer. Guide: Porosity and residual monomer
    • Resilient liners: silicone, or plasticized acrylic whose plasticizer leaches out so it hardens and roughens. Guide: Liners: hard relines, resilient liners and tissue conditioners
    • Acrylic teeth: chemical bond to the base but debond (22–30% of broken dentures), wear fast, wear opposing teeth less than porcelain. Guide: Denture teeth
    • Direct provisionals: PMMA 40.04 °C vs bis-acryl 39.16 °C mean pulp-chamber peak in one study; PMMA shrinks, leaches monomer, stains. Guide: Provisional crown materials

    Implant and endodontic materials

    • Titanium: grades 1 to 4 or alloys; oxide film in microseconds, 2 to 7 nm; still releases corrosion products and particles. Guide: Titanium for implants
    • Machined (turned) = grooves; grit-blasted = rough, better than machined; plasma-sprayed hydroxyapatite = bioactive coat. Guide: Implant surfaces
    • Zirconia implants: no gray shadow; transformation spreading through the surface (aging) is their risk. Guide: Zirconia implants
    • Gray through thin gingiva: often shine-through; titanium particles: metallosis; they look alike, so an unexplained dark macule is biopsied first. Guide: Gray or black around an implant
    • Gutta-percha: 19-22% trans-polyisoprene, 60-75% zinc oxide; cones β; α at 42-49 °C, amorphous with more heat; conducts heat poorly; shrinks on cooling. Guide: Gutta-percha
    • Sealers: ZOE (shrinks, decomposes when heated, eugenol hinders resin), epoxy resin (gold standard), methacrylate (Resilon, discontinued), hydraulic calcium silicate. Guide: Root canal sealers

    DentPrep · INBDE Dental Materials cheat sheet · dentprep.me/inbde

    Practice dental materials the exam's way.

    Your free account opens 100 INBDE questions with every option explained, and every subject's notes and cheat sheet.

    Start freeFree account · No card

    3 practice questions

    Three questions from the dental materials bank, each with its answer, why every other option is wrong, and its sources.

    Question 1 of 3

    What are the ADA's minimum requirements for a high noble casting alloy?

    1. ANoble metal ≥40 wt%, gold ≥25 wt%
    2. BNoble metal ≥60 wt%, gold ≥40 wt%
    3. CNoble metal ≥75 wt%, gold ≥60 wt%
    4. DNoble metal ≥25 wt%, no gold minimum
    Show the answer

    Answer BNoble metal ≥60 wt%, gold ≥40 wt%

    The ADA specification makes an alloy "high noble, with a noble-metal content of at least 60 wt% and a gold content of at least 40%" (Haugli 2020).

    Why the others are wrong

    • AThese numbers mix the thresholds; the high noble class needs 60% noble metal and 40% gold.
    • CThese figures exceed the minimums; the class needs only 60% noble metal and 40% gold. (Seventy-five percent or more of base metal describes alloys like cobalt-chromium, Al Jabbari 2014.)
    • DAt least 25% noble metal with no gold rule is the noble class.

    The rule (Haugli 2020): "The current ADA (American Dental Association) specification classifies dental alloys by composition, dividing alloys into three groups: (1) high noble, with a noble-metal content of at least 60 wt% and a gold content of at least 40%; (2) noble, with a noble-metal content at least 25% (no stipulation for gold); and (3) predominately base metal, with a noble-metal content less than 25%." The ADA proposed it in 1984 (Al Jabbari 2014).

    Class Noble metal Gold
    high noble at least 60 wt% at least 40 wt%
    noble at least 25 wt% no rule
    predominantly base metal less than 25 wt%

    Applied to the question: two conditions, both needed: 60% noble metal in total and 40% gold within it.

    Trap: an alloy rich in noble metals but with under 40% gold is noble, not high noble. Gold is the only metal with its own threshold.

    The point to rememberHigh noble: ≥60% noble metal and ≥40% gold; noble: ≥25%; predominantly base: <25%.

    Sources (2)
    1. Haugli KH, Syverud M, Samuelsen JT. Ion release from three different dental alloys: effect of dynamic loading and toxicity of released elements. Biomater Investig Dent. 2020;7(1) (PMC7241566), Introduction
    2. Al Jabbari YS. Physico-mechanical properties and prosthodontic applications of Co-Cr dental alloys: a review of the literature. J Adv Prosthodont. 2014;6(2):138 (PMC4024559), Introduction

    Question 2 of 3

    How did manufacturers make early polyvinyl siloxanes easier to pour without bubbles?

    1. AA tin catalyst in place of platinum
    2. BMore filler to raise the contact angle
    3. CSurfactants to lower the contact angle
    4. DSulfur compounds to speed the set
    Show the answer

    Answer CSurfactants to lower the contact angle

    "VPS materials were originally hydrophobic"; "efforts have been made to improve the hydrophilicity of VPS impression materials by adding external and/or internal surfactants to reduce contact angle and enhance wettability", and the surfactants "do not affect the physical properties of VPS" (Madanshetty 2023).

    Why the others are wrong

    • AAddition silicone's catalyst is chloroplatinic acid; changing the catalyst is not how wetting was improved.
    • BA higher contact angle means poorer wetting, the opposite of the aim.
    • DSulfur compounds poison the platinum catalyst and stop the set.

    The rule (Madanshetty 2023): "VPS materials were originally hydrophobic", which made bubble-free casts and void-free full-arch impressions hard to obtain. "Efforts have been made to improve the hydrophilicity of VPS impression materials by adding external and/or internal surfactants to reduce contact angle and enhance wettability. Although these surfactants reduce the surface tension of the liquid, they do not affect the physical properties of VPS," in the review's words.

    Contact angle Wetting
    high poor: gypsum beads up, voids form
    low (with surfactants) better: stone flows over the impression

    Applied to the question: a lower contact angle lets the wet stone spread over the impression's surface instead of trapping air.

    Trap: reading "hydrophilic" as "contains water". The surfactant changes how water spreads on the surface; the material is still an addition silicone.

    The point to rememberPVS was hydrophobic; surfactants lower its contact angle so the stone wets it.

    Sources (1)
    1. Madanshetty P, Guttal SS, Meshramkar R, Newaskar PS, Anehosur GV. Addition silicone impressions in fixed prosthodontics: clinical standpoints. Cureus. 2023;15(9):e44014 (PMC10517288), Hydrophilicity

    Question 3 of 3

    A ceramic onlay will be bonded with a resin cement at the next visit. Why is a noneugenol temporary cement usually advised for the provisional?

    1. AEugenol residue may inhibit resin polymerization
    2. BEugenol reacts with the onlay's hydrofluoric acid etch
    3. CNoneugenol cement bonds to the final ceramic
    4. DEugenol cement is too strong to remove
    Show the answer

    Answer AEugenol residue may inhibit resin polymerization

    "Caution has to be exercised when using eugenol-containing cements as the eugenol can contaminate the preparation. This can inhibit the polymerization of certain resin composites" (Pameijer 2012); "it is suggested to use zinc oxide non-eugenol as a temporary cement before the composite resin application" (Leung 2022).

    Why the others are wrong

    • BThe onlay is etched outside the mouth; the concern is eugenol on the tooth, where the resin must polymerize.
    • CThe provisional cement is removed before the onlay is bonded; it is not meant to bond to the final restoration.
    • DZinc oxide eugenol's "low strength allows for the easy removal of provisional crowns" (Leung 2022); strength is not the issue.

    The rule: "one common concern about zinc oxide eugenol is that eugenol hinders the polymerization of resin cement and leads to a reduced bond strength" (Leung 2022). The evidence is mixed: "several laboratory studies and a systematic review have shown that the use of eugenol-containing temporary cement does not alter the bond strength of resin" (Leung 2022). The cautious practice stands: a noneugenol temporary, and "Residual provisional cements should be thoroughly removed from the tooth before the application of final cements" (Heboyan 2023).

    Before an adhesive restoration
    provisional cement zinc oxide non-eugenol
    before bonding remove every trace of provisional cement

    Applied to the question: the onlay will depend on a resin cement polymerizing against that dentin, so nothing that may interfere with polymerization is left on it.

    Trap: knowing the debate and concluding eugenol is harmless. The question asks why the advice exists: eugenol may inhibit resin polymerization, and the noneugenol cement removes the doubt.

    The point to rememberResin bonding ahead: provisionalize with a noneugenol cement (eugenol may inhibit polymerization) and remove all of it.

    Sources (3)
    1. Pameijer CH. A review of luting agents. Int J Dent. 2012;2012:752861 (PMC3296365), 2.2 Provisional cements
    2. Leung GKH, Wong AWY, Chu CH, Yu OY. Update on dental luting materials. Dent J (Basel). 2022;10(11):208 (PMC9689175), 4.1 Zinc oxide eugenol and non-eugenol
    3. Heboyan A, Vardanyan A, Karobari MI, et al. Dental luting cements: an updated comprehensive review. Molecules. 2023;28(4):1619 (PMC9961919), 1. Introduction

    Take the free 20-question test →

    What the full guide covers

    The Dental Materials guide runs to about 18,000 words in 9 parts:

    1. Structure and properties
    2. Direct restorative materials and adhesion
    3. Liners, bases, pulp protection and preventive agents
    4. Luting cements
    5. Impression materials
    6. Alloys, casting and wire
    7. Ceramics
    8. Polymers for dentures and provisionals
    9. Implant, endodontic and laboratory materials

    The full notes and their PDF are free on a DentPrep account, beside the question bank.

    More INBDE subjects

    Clinical dentistry

    All 23 subjects →

    Free on your account

    100 INBDE questions, free.

    Every option explained, and every note, cheat sheet and PDF. Your free account never ends.

    One plan for all of it: $49 a month, $129 for three months, or $349 a year.

    Start freeFree account · No cardSee pricing
    What else your free account opens
    • Interviews5 scored answers, 1 mock interview with its report, and 2 Casper scenarios
    • TOEFLAll 20 lessons, one practice set of each Reading and Listening task, and 2 scored speaking or writing tasks
    • Application reviewYour first statement or resume review: the verdict, the summary, the strengths and the 2 most serious suggestions
    • Dental schoolFree: your lectures, summaries, questions and flashcards, 10 drafts and 10 summaries a day
    • School guidesAll 113, no account needed
    20 INBDE questions, free.Take the test